View Single Post
  #1 (permalink)  
Old 18-10-06, 08:39 PM
pelham939's Avatar
pelham939 pelham939 is offline
Senior Member
 
Join Date: Jun 2005
Location: Rotherham
Posts: 260
Gelcoat Catalyst

during my build i have done some running repairs and used gelcoat to get the colour built up but its still soft - i think i should have used a catalyst to finish the setting process - searched other threads and they confirm this - where do i get it from any glass fibre ditributor/supplier or is there a special?

thanks guys
__________________
Ian Gascoigne

Whether its broken or not fix it
Reply With Quote